Testing

The coupler was subjected to tensile force and the reinforcing bars were broken outside the coupler.

The Figure show sleeve half and two test specimens were subjected to tensile forces and the reinforcing bars were broken outside the coupler.

Introduction

First closure technique

Second closure technique

Third closure technique